Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® Clear G170 MED - PA* - ARKEMA

Material Data Center offers the following functions for Rilsan® Clear G170 MED:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Rilsan Clear datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
PA,,MT,C12-020

Rilsan® Clear G170 MED is a high performance transparent polyamide resin with outstanding thermal resistance. This grade offers the highest quality and is specifically designed to meet the stringent requirements of the medical applications.  Upon request letters regarding USP class VI  compliance can be provided.

Main applications:
  • Medical perfusion tube accessories
  • Breathing mask

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit,  please refer to our technical services.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 2 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 1.1 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.1 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 2100 / 2020 MPa ISO 527
Contrainte d'écoulement 76 / 74 MPa ISO 527
Déformation au seuil d'écoulement 8 / 9 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy (entaillé), +23°C - / 13 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C - / 13 kJ/m² ISO 179/1eA
Dureté Shore D 79 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 168 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 136 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 150 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 160 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 70 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-2 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Aptitude à l'allumage 26 / * % ISO 4589-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale - / 1E11 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E12 Ohm IEC 62631-3-2
Rigidité diélectrique - / 50 kV/mm IEC 60243-1
Indice de résistance au cheminement * / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 3.8 / * % Sim. to ISO 62
Absorption d'humidité 1.7 / * % Sim. to ISO 62
Masse volumique 1050 / 1050 kg/m³ ISO 1183
Fonctions
Viscosité / Vitesse de cisaillement , Rilsan® Clear G170 MED, PA*, ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Rilsan® Clear G170 MED, PA*, ARKEMA
Module de cisaillement dynamique / Température , Rilsan® Clear G170 MED (sec), PA*, ARKEMA
Module de traction dynamique / Température , Rilsan® Clear G170 MED (sec), PA*, ARKEMA
Contrainte / Déformation , Rilsan® Clear G170 MED (sec), PA*, ARKEMA
Module sécant / Déformation , Rilsan® Clear G170 MED (sec), PA*, ARKEMA
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Conditionnement
Granulés
Propriétés spéciales
Transparent
Certifications
Grade médical, USP Class VI approbation
Disponibilité régionale
Autres informations
Moulages par injection
Injection molding conditions:
- Typical melt temperature  (Min / Recommended / Max)  : 270°C / 290°C / 310°C.
- Typical mold temperature  : 40 - 80 °C.
- Dyring time and temperature (only for bags opened for more than two hours): 4 - 6 hours at 90°C.
Extrusion de films
 Extrusion conditions:
- Typical melt temperature  (Min / Recommended / Max)  : 270°C / 280°C / 290°C.
- Dyring time and temperature (only for bags opened for more than two hours): 4 - 6 hours at 90°C.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.